T304 Smls .188/.193” OD x .028”(+/-10%) wall annealed, Mil-T-8506 Tensile 80,000 to 100,000 PSI yield 41,000 to 51.000 PSI (aim for 46 KSI), elongation 30% minimum. Test and report all specs.
T304 Smls .188/.193” OD x .028”(+/-10%) wall annealed, Mil-T-8506 Tensile 80,000 to 100,000 PSI yield 41,000 to 51.000 PSI (aim for 46 KSI), elongation 30% minimum. Test and report all specs.