The presence of Iron in Aluminum aides in the decrease of hot tears, improves tensile, yield, and hardness and preserves strength at elevated temperature.
“281 to 338 ºF (138 to 170 ºC) Low Melting Point 60% Tin Cast Metal Alloys” has been added to your cart. View cart

Belmont Metals, Inc.