The presence of Iron in Aluminum aides in the decrease of hot tears, improves tensile, yield, and hardness and preserves strength at elevated temperature.
“136 ºF (58 ºC) Low Melting Point 49% Bismuth Alloys” has been added to your cart. View cart

Belmont Metals, Inc.
30% Ferrous and 70% Aluminum